Compression Strength of Borosilicate and Soda-Lime Silicate Glasses Using a Dumbbell Shaped Specimen
Report Number:
ARL-TR-9120
December 2, 2020
Approved for public release: distribution is unlimited.
Author(s):
Christopher S Meredith and Jeffrey J Swab
Abstract:The compression strength of a borosilicate and a soda-lime silicate glass is measured under quasi-static and dynamic strain rates with a dumbbell-shaped specimen. Two different specimen orientations were machined, parallel (vertical) and perpendicular (horizontal) to the plate thickness, and some specimens of each glass were etched prior to testing. A dumbbell specimen was used since the typical cuboid or cylindrical specimen develops a large stress concentration at the ends of the specimen, leading to premature failure and correspondingly low strength values. The dumbbell-shaped specimen allows one to differentiate between “valid” and “invalid” failure for each experiment by observing, with a high-speed camera, where fracture initiates—within the specimen gage section (valid) or from the specimen ends (invalid). However, damage can initiate in both the ends and the gage section (nearly) simultaneously, clouding the determination. Time correlating the force/stress measurement to the observed images has some uncertainty that can add additional ambiguity. The success rates for each glass were completely opposite: relatively high for borosilicate and very low for the soda-lime silicate. However, there is no obvious explanation. Despite these issues, it is believed that the dumbbell-shaped specimen is the best geometry for measuring the compression strength of brittle materials.